On wear model for piston ring and strengthened cylinder wall of engine  ( CPCI-S收录)  

文献类型:会议论文

英文题名:On wear model for piston ring and strengthened cylinder wall of engine

作者:Sun, Jian-min[1];Yang, Qing-mei[2]

第一作者:Sun, Jian-min

通讯作者:Sun, JM[1]

机构:[1]Beijing Univ Civil Engn & Architecture, Sch Mech Elect & Automobile Engn, Beijing 100044, Peoples R China;[2]Beijing Union Univ, Coll Automat, Beijing 100101, Peoples R China

第一机构:Beijing Univ Civil Engn & Architecture, Sch Mech Elect & Automobile Engn, Beijing 100044, Peoples R China

通讯机构:[1]corresponding author), Beijing Univ Civil Engn & Architecture, Sch Mech Elect & Automobile Engn, Beijing 100044, Peoples R China.

会议论文集:9th International Conference on Engineering Structural Integrity Assessment

会议日期:OCT 15-19, 2007

会议地点:Beijing Univ Aeronaut & Astronaut, Beijing, PEOPLES R CHINA

主办单位:Beijing Univ Aeronaut & Astronaut

语种:英文

摘要:Ni-P electroless plating is applied to repairing engine cylinder is advanced. For practical operation conditions of engine cylinder, piston speed and lateral pressure to cylinder wall are determined as experimental factors, and abrasion value of cylinder is set as wear resistance target. According to load and speed on 1mm similar to 8mm below top dead center of cylinder in expansion stroke, the ranges of experimental parameters are chosen. Based on the quadratic regression rotation combination method, wear resistance experiment of hardening material is designed. The wear mathematic models of Ni-P electroless plating is established, and three-dimensional curved surfaces for load-speed-wearing value are drawn. The results show that the Ni-P electrolessl plating is fit for the operating condition of cylinder, and can increase relative wear resistance of cylinder by 5 times. By analysis of wear mechanisms of hardening material and wear resistance, the material is perfect for hardening engine cylinder wall.